Material data

Typical properties

92N75 — Typical properties
Test ItemsTest Method92N75
Hardness, Shore (A)ASTM D224075
Density (g/cm³)ASTM D7920.98
MFR,230℃,5kg(g/10min)ASTM D41215
Tensile Strength (MPa)ASTM D4128
Elongation (%)ASTM D412500
Tear Strength (kN/m)ASTM D62432
Compression Set 70℃/22h (%)ASTM D39542
Brittle point (℃)ASTM D746-55
Processing temperature (℃)—180-220